In our country, high purity magnesite was tried to burn by oil shaft kiln and turned to merchandise in eighties , but the output is small , Almost in the meantime ,coke shaft kiln further burned middle grade mag - nesite were launch, but burned with coke could increase the silicon but depress magnesite's grade low, so we built middle grade magnesite oil shaft kiln.
Index | MgO%≥ | SiO2 %≤ | CaO %≤ | B.D. | LOI |
TMS-95A | 95 | 1.4 | 1.6 | 3.26 | 0.3 |
TMS-95B | 94.5 | 1.6 | 1.8 | 3.25 | 0.3 |
TMS-95A | 95 | 2.0 | 1.6 | 3.20 | 0.3 |
TMS-94B | 94.5 | 2.5 | 1.8 | 3.20 | 0.3 |